Clues for die wear. (On the pre single squeeze dies)1. the fields are showing flow lines.
2. The outside edge near the rims will be weaker/mushy like being distorted.
3. The devices move towards the rims as the die ages even more.
Single squeeze dies with DDD:1. The fields are affected, not the devices.
2. After this sets in the
Ridge Ring is next noted.