I had a similar 87D earlier today. I could see clear past the plating to the void below. Once the copper splits, the substrate (zinc) is subject to the elements. Eventually, hydrozincite sets in (under magnification, it looks like bright white cauliflower). Since the zinc is consumed, the void is left and the copper collapses in.